Polishing rods for strength
When smoothing the casting ridge on cast small block rods should you smooth the entire side of the rod down so it is flush or just polish the very top of the casting ridge?
__________________
Vehicle Repair/Maintenance and TIG welding services for hire (steel and Aluminium), PM or IM me
AIM: Acidtalons
Vehicle Repair/Maintenance and TIG welding services for hire (steel and Aluminium), PM or IM me
AIM: Acidtalons
talking bout this here.
Casting ridge is an easy place for a crack to start and if it spreads then the rest of the rod will break.
Just not sure how much to smooth off.
Casting ridge is an easy place for a crack to start and if it spreads then the rest of the rod will break.
Just not sure how much to smooth off.
__________________
Vehicle Repair/Maintenance and TIG welding services for hire (steel and Aluminium), PM or IM me
AIM: Acidtalons
Vehicle Repair/Maintenance and TIG welding services for hire (steel and Aluminium), PM or IM me
AIM: Acidtalons
Last edited by Acidtalons; Dec 22, 2003 at 11:23 PM.